For Low Resilience Foam Applications
Introduction
KONIX SR-308 is for low resilience foam.
Typical Properties
| Color (APHA) | 50 max |
| Hydroxyl Number (mgKOH/g) | 293.0-323.0 |
| Acid Number (mgKOH/g) | 0.05 max |
| PH | 5.0-7.5 |
| Moisture Content (%) | 0.05 max |
| Viscosity, cps, 25°C | 265-305 |
Applications
KONIX SR-308 can be used to produce bed mats material, toys, etc.
Storage
KONIX SR-308 need to be stored in a ventilated storage area below 50°C, keep container closed to product from moisture contamination. Use only with adequate ventilation.
Handling Precautions
KONIX SR-308 may cause slight skin or eye irritation upon contact. Inhalation hazard is not anticipated at normal temperature.